Gagne de la cryptomonnaie GRATUITE en 5 clics et aide institut numérique à propager la connaissance universitaire >> CLIQUEZ ICI <<

Références bibliographiques

Non classé

[1] Donald M.Matox, Handbook of Physical Vapor Deposition (PVD) Processing (Second Edition), Elsevier inc. 2010.
[2] Donald M.Matox, The foundations of vacuum film technology, William Andrew publishing 2003.
[3] Alain Cornet, Jean-Paul Deville, Physique et ingénierie des surfaces, Monographie de matérialogie 3.
[4] Krishna Seshan, Handbook of Thin Film Deposition Processes and Techniques second edition, William Andrew publishing 2002.
[5] Donald M.Matox, Atomistic Film Growth and Some Growth-Related Film Properties, Handbook of physical vapor deposition, pages 366-398.
[6] Stojan S.Djokic, Electrodeposition, Structure, NY Springer 2010.
[7] Petrova, P. B. Barna, L. Hultman, J. E. Greene, Journal of Vacuum Science and Technology, 21 (2003) 5.
[8] J.M. Lacknera, W. Waldhausera, B. Majorb, J. Morgielb, L. Majorb et H. Takahashic, T. Shibayamac, Surface and Coatings Technology 200 (2006) 3644–3649.
[9] B. Borer, A. Sonnenfeld, Ph. Rudolf von Rohr, Surface and Coatings Technology 201 (2006) 1757-1762.
[10] R. Messier, S. Trolier-McKinstry, Journal of Vacuum Science and Technology (2001) 9306-9313.
[11] Donald M.Matox, Thin Solid Films, 53 (1978) 81-96.
[12] P.K. Srivastava, V.D. Vankar, K.L. Chopra, Bulletin of Material Science Vol 8 No.3 (1986) 379-384.
[13] K. Abdelouahdi, Surface and Coating Technology, 200 (2006) 6469-6473.
[14] Kiyotaka Wasa, Makoto Kitabatake, Hideaki Adachi, Thin Film Materials technology, (2004) 17-67.
[15] H.O Pierson, Handbook of Refractory Carbides and Nitrides, (1996) 100-117.
[16] Erwin Rudy, Journal of the less common metals, 33 (1973) 245-273.
[17] E. RUDY, Compendium of phase diagram data, U.S Air Force technical report AFML-TR-65-2, PART V, 1969, 192-197.
[18] B. Uhrenius, Calphad, Vol. 8 No. 2 1984, 101-119.
[19] P.Gustafson, Materials Science and Technology, 2, (1986) 653-658.
[20] Marios D. Demetriou, Nasr M. Ghoniem, Adrienne S. Lavine, Computation of metastable phase in tungsten-carbon system, Mechanical and Aerospace Eng. Dep, University of California, Los Angeles CA 90095-1597.
[21] Kiyotaka Wasa, Makoto Kitabatake, Hideaki Adachi, Thin films materials technology, (2004), 191-403.
[22] A. Cavaleiro, M. T.Viera, Thin Solid Films, 185 (1990) 199-217.
[23] E. Krzanowski, Jose, L. Endrino, Materials Letters, 58 (2004) 3437-3440.
[24] E. Eser, R. E.Ogilvie, K. A.Taylor, Thin Solid Films, 67 (1980) 265-277.
[25] E. Raekelboom, K. Abdelouahdi, C. Legrand-Buscema, Thin Solid Films, 517 (2009) 1555–1558.
[26] J.J. Cuomo, R. J. Gambino, R. Rosenberg, J. Vac. Sci. Technol., 11 (1974) 34.
[27] M. Gubisch, Y. Liu, S. Krischok, G. Ecke, L. Spiess, J.A. Schaefer, C. Knedlik, Life Cycle Tribology, (2005) 409.
[28] J.P. Palmquist, Zs. Czigany, M. Odén, J. Neidhart, L. Hultman, U. Jansson, Thin Solid Films, 444 (2003) 29-37.
[29] I.A. Ryabchikov, S.V. Dektyarev, I.B. Stepanov, Surface and Coatings Technology, 201 (2007) 6526–6529.
[30] A. Cavaleiro and M. T. Vieira, Thin Solid Films, 213 (1992) 612.
[31] B.R. Pujada, G. C.A.M. Janssen, Surface and Coatings Technology, 201 (2006) 4284-4288.
[32] B. G. Wagh, V. P. Godbole ,S. B. Ogale, Surface and Coatings Technology, 49 (1991) 439-442.
[33] K. Fuchs, P. Rodhammer, E. Bertel, F. P. Netzer, et E. Gornik, high rate sputter deposition of WC, (1987) 383-395.
[34] K. Abdelouahdi, C. Sant, C. Legrand-Buscema, P. Aubert, J. Perrière, G. Renou et Ph. Houdy, Surface and Coatings Technology 200 (2006) 6469-6473.
[35] A. Lousa, C. Rincon, J. Romero, J. Esteve, E. Martinez, Surface and Coatings Technology 163 –164 (2003) 386-391.
[36] P. K. Srivastava, V. D. Vankar, K. L. Chopra, Thin Solid Films, 161 (1988) 107-116.
[37] A. Cavaleiro, E. Costa, Surface and Coatings Technology, 97 (1997) 680-686.
[38] C. Strondl, N. M. Carvalho, J .Th.M. De Hosson, G.J. van der Kolk, Surface and Coating Technology, 162 (2003) 288.
[39] C. Strondl, N. M. Carvalho, J. Th. M. De Hosson, T. G. Krug, Surface and Coating Technology, 200 (2005) 1142.
[40] G. Zambrano, P. Prieto, F. Perez, C. Rincon, H. Galindo, L. Cota-Araiza, J. Esteve, E. Martinez, Surface and Coatings Technology, 108–109 (1998) 323-327.
[41] H. Yueh Yang, X. A. Zhao, M. A. Nicolet, Thin Solid Films, 158 (1988) 37-44.
[42] André Anders, Thin Solid Films, 518 (2010) 4087-4090.
[43] Yong Seob Park, Young Park, Hosung Jung, Tae-Hwan Jung, Dong-Gun Lim, Won Seok Choi, article in press TSF-30358, Thin Solid Films No of Pages 5.
[44] Jyh-Wei Lee, Yu-Chu Kuo, Chaur-Jeng Wang, Li-Chun Chang, Kuan-Ting Liu, Surface and Coatings Technology, 203 (2008) 721-725.
[45] M. Ahlgren, H. Blomqvist, Surface and Coatings Technology, 200 (2005) 157– 160.
[46] K. Chu, P.W. Shum, Y.G.Shen, Materials Science and Engineering, 131 (2006) 62–71.
[47] Maria Nordin, Mats Larsson, Surface and Coatings Technology, 116–119 (1999) 108–115.
[48] Deepak G. Bhat, Robert A. Holzl, Thin Solid Films, 95, 2 (1982) 105-112.
[49] P.Q. Wu, D. Drees, L. Stals, J. P. Celis, Surface and Coatings Technology, 113, 3 (1999) 251–258.
[50] B.M. Kramer, P. K. Judd, Journal of Vacuum Science and Technology, A, 3, 6 (1985) 2439.
[51] J.E. Sundgren, H.T.G. Hentzell, Course on Vapour Deposited Wear Protective Coatings, Continuing Education Institute, Miltenberg, October 6-9, 1986, CEI-Europe, Finspang, Sweden, 1986, Chapter 1.
[52] B.C. Schramm, H. Scheerer, H. Hoche, E. Broszeit, E. Abele, C. Berger, Surface and Coatings Technology, 188–189 (2004) 623– 629.
[53] Junhu Xu, Hiroyuki Umehar, Isao Kojim, Applied Surface Science, 201 (2002) 208–218.
[54] J.L. Mo, M.H. Zhu, B. Lei, Y.X. Leng, N. Huang, Wear, 263, 7–12 (2007), 1423–1429.
[55] A.A. Voevodin, M.S. Donley, J.S. Zabinski, Surface and Coatings Technology, 92, 1–2 (1997), 42-49.
[56] Michael E. O’Hern, Robert H. Parrish, Warren C. Oliver, Thin Solid Films, 181 (1989) 357-363.
[57] K.A. Taylor, Thin Solid Films, 40 (1977) 201-209.
[58] A. Ramalho, A. Cavaleiro, A.S. Miranda, M.T. Vieira, Surface and Coatings Technology, 62 (1993) 536-542.
[59] J. Esteve, G. Zambrano, C. Rincon, E. Martinez, H. Galindo, P. Prieto, Thin Solid Films, 373 (2000) 282-286.
[60] K. Bewilogua, H. Dimigen, Surface and Coatings Technology, 61 (1993) 144-150.
[61] S.Ramalingam, W.O Winer, Thin Solid films, 73 (1980) 267-274.
[62] Biophyresearch.com/spectroscopie.auger.pdf.
[63] M. Gubisch, Al., Thin Solid Films, 488 (2005) 132-139.
[64] Thèse de doctorat, Anne-Sophie LOIR, Élaboration de couches minces de carbone par ablation laser femtoseconde pour application aux biomatériaux implantables.
[65] C.Reynaud, Journal os Science and Interface Analysis, Ecasia 01 (2001)
[66] F. Ng-Cheng-Chin, M. Roslin, Z. H. Gu., T. Z. Fahidy, J. Phys. D Appl. Phys., 31 (1998).
[67] L. A. Goodman, RCA Rev., 35 (1974) 613.
[68] C. M. Lampert. Sol. Energy Mater, (1981) 6-11.
[69] P.O. Renault, D. Faurie, E. LE Bourhis, PH. Goudeau, P. Villain, Lab. Métallurgie.
Physique – UMR 6630 CNRS/Univ. Poitiers, SP2MI, P 30179, 86962 Futuroscope.
[70] J. D. Mac Brayer, R. M. Swanson and T. W. Sigmon, J. Electrochem. Soc., Solid State Science and Technology 133(6) (1986) 1243.
[71] K. Abdelouahdi, C. Sant, C. Legrand-Buscema, P. Aubert, J. Perrière, G. Renou, Ph. Houdy, Surface and Coatings Technology 200 (2006) 6469-6473.
[72] La Société Française de Métallurgie et Matériaux Section Ouest, Colloque SF2M.
[73] Section-Ouest : Surfaces et Interfaces, indentation, rayage et abrasion, Angers 2005.
[74] S.Lecume, C.Spykerelle, F.Sommer, Structure of pristine crystal defects revealed by AFM and microtomography, Abstracts APS, 2003, USA.
[75] www.Biophyresearch.com/MEB.pdf
[76] Cours Microscopie électronique à transmission et ses techniques d’analyses, J. Ghanbaja, Service Commun des Microscopies Electroniques et Microanalyses X, Nancy université.
[77] Thèse de doctorat, Zhonghuai WANG, Développement d′un Microscope à Force Atomique Multifonctionnel Associé à un Microscope Electronique à Balayage, Université de Reims.
[78] H. Bückle, in J.W. Westbrook, H. Conrad (Eds.), The Science of Hardness Testing and its Applications, American Society for Metals, Metals Park, OH, (1973) 453.
[79] H. Hertz ; Über die Berührung fester elastische Köper. J. Reine und angewandte Mathematik, 92 (1882) 156-171.
[80] H. Hertz; on the contact of elastic solods. J Reine Angew Math 92 (1881) 156-171. Translated and reprinted in English. In Hertz’s miscellaneaous papers. London: Macmillan and Co., 1896 [chapter 5].
[81] H. Hertz; On hardness. Verch Ver Beforderung Gewerbe Fleisses 61 (1881) 410. Translated and reprinted in English. In Hertz’s miscellaneaous papers. London: Macmillan and Co., 1896 [chapter 6].
[82] I. N. Sneddon, the relation between load and penetration in the axisymmetric Boussineq problem for a punch of arbitrary profile; Int. J. Eng. Sci. 3 (1965) 47.
[83] S.I. Bulychev, V.P. Alekhin, M.Kh. Shorshorov, A.P. Ternovskii, and G.D. Shnyrev, Zavod. Lab. 41, (1975) 1137.
[84] S.I. Bulychev, V.P. Alekhin. M.Kh. Shorshorov, and A.P . Ternovskii, Prob. Prochn. 9 (1976) 79.
[85] M.Kh. Shorshorov, S.I. Bulychev. And V.P. Alekhin, Sov. Phys. Dokl., 26 (1982) 769.
[86] S.I. Bulychev and V.P. Alekhin, Zavod, Lab. 53, (1987) 76.
[87] M.F. Doerner, W.D. Nix, « A method for interpreting the data from depth-sensing indentation instruments », Journal of Material Research, 1(4) (1986) 601-609.
[88] W.C. Oliver, R. Hutchings, J.B Pethica, ASTM STP 889, édité par P.J Blau and B.R Lawn (American Society for Testing and Materials, Philadelphia, PA, 1986) 90-108.
[89] W.C. Oliver, G.M. Pharr, « An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments », Journal of Material Research, 7 (6) (1992) 1564-1583.
[90] W.C. Oliver, G.M. Pharr, « Measurement of hardness and elastic modulus by instrumented indentation. Advances in understanding and refinement methodology », Journal of Materials Research, 19(1) (2004) 3-20.
[91] R.B. King. Elastic analysis of some punch problems for layered medium, International Journal of Solids and Structures, 23(12) (1987) 1657-1664.
[92] D. Tabor, Clarendon Press, Oxford, 1951.
[93] T.Y. Tsui, G.M. Pharr, Journal of Material Research,, Substrate effet on nanoindentation mechanical property measurement of soft films on hard substrates. 14(1) (1999) 292-301.
[94] Cheng Y.T., Cheng C.M., elastic modulus and the work of indentation. Applied Physics Letters, 73(5) (1998) 614-616.
[95] A. Bolshakov, G. M. Pharr, Journal of Materials Research 13 (4) (1998) 1049-1058.
[96] T. Chudoba, F. Richter, Surface and coating technology, 148 (2001) 191-198.
[97] J.S. Field, M.V. Swain. A simple predictive model for spherical indentation. Journal of Material Research, Vol. 8 N.2 1993.
[98] S. Suresh, T.G. Nieh, B.W. Choi, Nanoindentation of copper thin films on silicon substrates, Scripta Materialia, Vol. 41, No. 9, 951–957, 1999.
[99] A. Gouldstone, H.J. Koh, K.Y. Zeng, A.E. Giannakopoulos, S. Suresh, « Discrete and continuous deformation during nanoindentation of thin films », Acta Materialia. 48 (2000) 2277-2295.
[100] François Robe Valloire, René Gras, Tribologie et conception mécanique, Press polytechniques et universitaires romande.
[101] Xiaodong Li, Bharat Bhushan. Materials Characterization, 48 (2002) 1136.
[102] Thèse de doctorat à l’École des Mines de Paris, Sébastien ROY, Mesure de l’adhérence et des propriétés mécaniques de couches minces par des essais dérivés de la nanoindentation, Application à la microélectronique et au biomédical (2008).
[103] D. S. Rickerby, Surface and Coatings Technology 36 (1988) 541-557.
[104] S.J. Bull, E.G. Berasetegui, An overview of the potential of quantitative coating adhesion measurement by scratch testing, Tribology International, 39,2 (2006), 99-114.
[105] P.J. Burnett, D.S. Rickerby, Thin Solid Films, 15 (1987) 403-416.
[106]S. J. Bull, Tribology International, 30 (1997) 491-498.
[107] L.W. Ma, J.M. Cairney, M.J. Hoffman, P.R. Munroe, Surface and Coatings Technology, 204 (2010) 1764–1773.
[108] P.A. Steinmann, Y. Tardy, H.E. Hintermann, Thin Solid Films, 154 (1987) 333-349.
[109] Jianliang Lin, William D. Sproul, John J. Moore, Surface and Coatings Technology, 206 (2012) 2474–2483.
[110] C. Subramanian, K. N. Strafford , T. P. Wilks , L. P. Ward , W. Mc Millan, Surface and Coatings Technology, 62 (1993) 529-535.
[111] P.R. Chalker, S.J. Bull, D.S. Rickerby, Materials Science and Engineering , A, Volume 140, (1991) 583-592.
[112] A.J. Perry, J. Valli, P.A. Steinmann, Surface and Coatings Technology, 36, 1-2 (1988) 559-575.
[113] N. X. Randall, G. Favaro, C.H. Frankel, Surface and Coatings Technology, 137 (2001) 146-151.
[114] H. Ichimura, Y. Ishii, Surface and Coatings Technology, 165 (2003) 1-7.
[115] E. Costa, A. Cavaleiro, Surface and Coatings Technology, 97 (1997) 680–686.
[116] C. Rincon, J. Romero, J. Esteve, E. Martinez, A. Lousa, Surface and Coatings Technology 163-164 (2003) 386-391.
[117] A. Ramalho, A. Cavaleiro, A. S. Miranda, M. T. Vieira, Surface and Coatings Technology, 62 (1993) 536-542.
[118] J.M. Castanho, M.T. Vieira, Surface and Coatings Technology 102 (1998) 50-62.

Page suivante : Annexe 1. Calcul de la fonction d’aire de contact

Retour au menu : CARACTERISATION MECANIQUE ET ADHERENCE DE REVETEMENT PVD EN CARBURE DE TUNGSTENE